Do not rush this. Most high-strength epoxies require 24 to 48 hours to fully cure. Exposure to water before it is fully hardened will cause the repair to fail immediately. Testing the Repair
Tub replacement parts are expensive, often costing 50% of a new machine. If the epoxy fix fails, it is usually time to replace the appliance. Washing Machine Cracked Tub Repair
Sand the area around the crack (about 2 inches in every direction) to "rough up" the plastic. Do not rush this
Small hairline cracks or pinholes in plastic (polypropylene) tubs can often be sealed. Washing Machine Cracked Tub Repair